AWS B2.1: 2005 Specification for Welding Procedure and Performance Qualification
276 стр.
An American National Standard
Approved by the American National Standards Institute
November 5, 2004
This specification provides requirements for the qualification of welding procedures. It also provides requirements for the performance qualification of welders and welding operators. This specification is intended for use where referenced by a product or fabrication code, specification, contract document, or inteal documents such as quality control or quality assurance manuals. The requirements imposed by the Referencing Document (see 1.3.2 Supplemental Definitions) supersede the requirements of this specification. This specification is intended for use with the following welding processes:
OFW = Oxyfuel Gas Welding
SMAW = Shielded Metal Arc Welding
GTAW = Gas Tungsten Arc Welding
SAW = Submerged Arc Welding
GMAW = Gas Metal Arc Welding
FCAW = Flux Cored Arc Welding
PAW = Plasma Arc Welding
ESW = Electroslag Welding
EGW = Electrogas Welding
EBW = Electron Beam Welding
LBW = Laser Beam Welding
SW = Stud Arc Welding
Appropriate metric conversions are included for all dimensions. However, the customary units are standard units, and the metric units are for information only. It is intended that inspection of qualification test welds is to be accepted based on the U.S. customary dimensions, not on the metric conversion values of these dimensions.
Возможность скачивания данного файла заблокирована по требованию правообладателя.
Смотрите также

API RP 2201 - 1995 Procedures for Welding or Hot Tapping on Equipment in Service (Eng)

Стандарт
  • формат pdf
  • размер 215.43 КБ
  • добавлен 18 января 2012 г.
American Petroleum Institute (API) Fourth Edition, September 1995. 23p. This publication covers the safety aspects to be considered when hot tapping, or when welding without hot tapping on in-service piping or equipment. It is not a substitute for job planning. A detailed, written procedure for hot tapping and welding should be prepared or reviewed before starting each job to ensure that all proper steps are taken.

API RР 577-2004 Welding Inspection and Metallurgy (Eng)

Стандарт
  • формат pdf
  • размер 5.86 МБ
  • добавлен 17 января 2012 г.
American Petroleum Institute (API). First Edition. October 2004. 114p. This recommended practice (RP) provides guidance to the API authorized inspector on welding inspection as encountered with fabrication and repair of refinery and chemical plant equipment and piping. Common welding processes, welding procedures, welder qualifications, metallurgical effects from welding, and inspection techniques are described to aid the inspector in fulfilling...

API Spec 16A-1997 Specification for Drill Through Equipment

Стандарт
  • формат pdf
  • размер 5.97 МБ
  • добавлен 13 декабря 2011 г.
67 стр. American Petroleum Institute, Second Edition, December, 1997 This specification is formulated to provide for the availability of safe and functionally interchangeable drill through equipment utilized for drilling for oil and gas. Technical content provides requirements for performance, design, materials, tests and inspection, welding, marking, handling, storing, and shipping. This specification does not apply to field use or field testing...

API Spec 16С-1993 Specification for Choke and Kill Systems

Стандарт
  • формат pdf
  • размер 3.94 МБ
  • добавлен 13 декабря 2011 г.
63 стр. American Petroleum Institute, First Edition, Januaru, 1993 This specification was formulated to provide for safe and functionally interchangeable surface and eubsea choke and kill systems equipment utilized for drilling oil and gas wells. Other parts of the Choke and ЮН System not specifically addressed in this document shall be in accordance with the applicable sections of this specification. Technical content provides the minimum requir...

API Spec Q1 Specification for Quality Programs for the Petroleum and Natural Gas Industry

Стандарт
  • формат pdf
  • размер 1.18 МБ
  • добавлен 03 декабря 2011 г.
20 cтр. API SPECIFICATION Q1 SIXTH EDITION, MARCH 1, 1999 EFFECTIVE DATE: SEPTEMBER 1, 1999 API Specification Ql provides requirements for a quality system that may be applied on an international basis to facilitate the consistent and reliable manufacture of products to specifications prepared for the oil and gas industry. Part One of this Standard is aligned with ANSI/ISO/ASQC Q9001- 1994, Quality Systems—Model for Quality Assurance in Design, D...

AWS B4.0: 2007 Standard Methods for Mechanical Testing of Welds

Стандарт
  • формат pdf
  • размер 3.09 МБ
  • добавлен 09 декабря 2011 г.
154 стр. An American National Standard Approved by the American National Standards Institute May 2, 2007 7th Edition This specification establishes standard methods for mechanical testing of welds. The significance of each test, test apparatus, preparation of the test specimens, and the test procedure are described. Example test results sheets are provided. It is beyond the scope of this document to define the required mechanical properties or ac...

AWS D1.1/D1.1M: 2010 Structural Welding Code - Steel

Стандарт
  • формат pdf
  • размер 19.75 МБ
  • добавлен 09 декабря 2011 г.
569 стр. An American National Standard Approved by the American National Standards Institute March 11, 2010 22nd Edition This code contains the requirements Tor fabricating and erecting welded steel structures. When this code is stipulated in contract documents, conformance with all provisions of the code shall be required, except for those provisions that the Engineer (see 1.4.1) or contract documents specifically modifies or exempts. The follow...

BS EN 12953-11: 2003 Shell boilers - Part 11: Acceptance tests (Eng)

Стандарт
  • формат pdf
  • размер 560.33 КБ
  • добавлен 18 декабря 2011 г.
This European Standard was approved by CEN on 24 July 2003. 36p. This Part of this European Standard specifies a concise procedure for conducting thermal performance tests, using the indirect (losses) procedure for boilers for steam or hot water. Test results are based on either the gross or net calorific value of the fuel.

Siemens. UL 1449 Third Edition

Стандарт
  • формат pdf
  • размер 1.2 МБ
  • добавлен 15 ноября 2011 г.
2 страницы SPD/TVSS Changes Effective September 29, 2009 UL 1449 has undergone extensive revision as surge suppression’s standard for safety. UL 1449 Third Edition, defines performance testing and nomenclature, which effectively reboots the surge industry. UL 1449’s performance testing provides a way to compare newly evaluated Surge Protective Devices (SPDs), formerly known as Transient Voltage Surge Suppressors (TVSS). These changes became effec...